Products
Contact Us




ATR (Attenuated Total Reflection)
Category:
Diamond, with its high hardness and resistance to acids, alkalis, and chemical corrosion, along with its high infrared transmittance, is renowned as the optimal ATR (Attenuated Total Reflection) crystal. Compared to other crystal materials, diamond ATR components withstand higher pressures, provide closer contact between samples and the crystal, achieve deeper penetration depth, and yield superior infrared spectra. Our company offers customized diamond ATR components in various shapes and specifications, ensuring materials and products adhere to rigorous control standards.
Product Description
Diamond ATR components
Main Parameter
● Spectral Range: 4500-2300 cm-1; 1800-400 cm-1
● Refractive Index: 2.42
● Total Internal Reflection Angle: 24.5°
● Penetration Depth: 2.01 μm (1000 cm-1, 45°)
● pH Range: 1-14
● Melting Point: 3550°C
● Thermal Conductivity: >2000 W/mK
● Coefficient of Thermal Expansion: 1.0 ppm/K
● Hardness (Mohs Scale): 10